Related Posts Plugin for WordPress, Blogger...

Thursday, April 12, 2012

Wednesday, April 11, 2012

Tuesday, April 10, 2012

Scheveningen - Beach

Neopan 400 -->200 asa, Tanol
Easy Lith: 30A-30B-1000 water + 100ml Old Brown
Exp. 50 sec. F/5,6
Lith developing: 4 min.



                                 Swefel Toner                                        Gold toner

Thursday, February 23, 2012

Run to you

Lith SE5 40A + 40B + 1500ml water + 100 old lith
Exp. F/8 80sec
Lith developing for 8.20
Gold toning (18-1) for 1 

Thursday, February 16, 2012

Sunday, February 12, 2012

The Art of Waiting

Negative Neopan 400 asa
In Tanol
Moersch Lith SE5
40+40+1500water + 100 old brown
(leftover from the last Lith session)
Exp. 40 sec. on F/4.5  Lith dev. 5.20 min.




Friday, February 10, 2012

Kralingse plas in Lith

Moersch SE5 Lith: 30A + 30B + 1000 water
Exposure of the negative: between 35 and 45 sec.
Lith development: between 4 and 15 min.
Old Agfa Record Rapid paper